Intergranular corrosion of Cu-Al-Ni alloy in 0.5 mol dm−3 H2SO4 solution

The corrosion behaviour of Cu-Al-Ni alloy in 0.5 mol dm–3 H2SO4 solution was investigated by electrochemical methods including open circuit potential measurement, electrochemical impedance spectroscopy measurements, linear and potentiodynamic polarization. Measurements were performed in 0.5 mol dm–3...

Full description

Permalink: http://skupnikatalog.nsk.hr/Record/nsk.NSK01001098225/Details
Matična publikacija: Kemija u industriji (Online)
69 (2020), 9/10 ; str. 457-464
Glavni autori: Vrsalović, Ladislav (Author), Gudić, Senka, Terzić, Lana, Ivanić, Ivana, inženjerka metalurgije, Kožuh, Stjepan, Gojić, Mirko, Oguzie, Emeka Emmanuel
Vrsta građe: e-članak
Jezik: eng
Predmet:
Online pristup: https://doi.org/10.15255/KUI.2020.022
Kemija u industriji (Online)
Hrčak
LEADER 03166naa a22004454i 4500
001 NSK01001098225
003 HR-ZaNSK
005 20210611104122.0
006 m d
007 cr||||||||||||
008 210420s2020 ci ad |o |0|| ||eng
024 7 |2 doi  |a 10.15255/KUI.2020.022 
035 |a (HR-ZaNSK)001098225 
040 |a HR-ZaNSK  |b hrv  |c HR-ZaNSK  |e ppiak 
041 0 |a eng  |b eng  |b hrv 
042 |a croatica 
044 |a ci  |c hr 
080 1 |a 66  |2 2011 
080 1 |a 669  |2 2011 
100 1 |a Vrsalović, Ladislav  |4 aut 
245 1 0 |a Intergranular corrosion of Cu-Al-Ni alloy in 0.5 mol dm−3 H2SO4 solution  |h [Elektronička građa] /  |c Ladislav Vrsalović, Senka Gudić, Lana Terzić, Ivana Ivanić, Stjepan Kožuh, Mirko Gojić, Emeka Emmanuel Oguzie. 
300 |b Ilustr. ; graf. prikazi. 
504 |a Bibliografija: 31 jed. 
504 |a Abstract ; Sažetak. 
520 |a The corrosion behaviour of Cu-Al-Ni alloy in 0.5 mol dm–3 H2SO4 solution was investigated by electrochemical methods including open circuit potential measurement, electrochemical impedance spectroscopy measurements, linear and potentiodynamic polarization. Measurements were performed in 0.5 mol dm–3 H2SO4 at temperatures 20 and 40 °C. After polarization testing, corroded electrode surfaces were ultrasonically cleaned in deionized water and examined by light and scanning electron microscopy, while the elemental composition at individual points of the alloy surface was determined by EDS analysis. The results of the investigations revealed the occurrence of intergranular corrosion on the Cu-Al-Ni surface, which became more pronounced with increasing temperature. 
520 |a Korozijsko ponašanje Cu-Al-Ni legure u 0,5 mol dm–3 H2SO4 otopini ispitivano je elektrokemijskim metodama kao što su mjerenje potencijala otvorenog strujnog kruga, mjerenje metodom elektrokemijske impedancijske spektroskopije, linearne i potenciodinamičke polarizacije. Mjerenja su provedena u 0,5 mol dm–3 H2SO4 pri temperaturama od 20 i 40 °C. Nakon polarizacijskih mjerenja korodirane površine elektroda ultrazvučno su očišćene u deioniziranoj vodi i ispitane svjetlosnim i pretražnim elektronskim mikroskopom, dok je elementarni sastav na pojedinim točkama na površini određen EDS analizom. Rezultati ispitivanja pokazali su da dolazi do interkristalne korozije na površini Cu-Al-Ni legure, čiji intenzitet raste s povećanjem temperature elektrolita. 
653 0 |a Legure  |a Korozija  |a Polarizacija  |a SEM/EDS 
700 1 |a Gudić, Senka  |4 aut 
700 1 |a Terzić, Lana  |4 aut 
700 1 |a Ivanić, Ivana,  |c inženjerka metalurgije  |4 aut 
700 1 |a Kožuh, Stjepan  |4 aut 
700 1 |a Gojić, Mirko  |4 aut 
700 1 |a Oguzie, Emeka Emmanuel  |4 aut  |9 HR-ZaNSK 
773 0 |t Kemija u industriji (Online)  |x 1334-9090  |g 69 (2020), 9/10 ; str. 457-464  |w nsk.(HR-ZaNSK)000530475 
981 |b Be2020  |b B03/20 
998 |b tino2106 
856 4 0 |u https://doi.org/10.15255/KUI.2020.022 
856 4 0 |u http://silverstripe.fkit.hr/kui/issue-archive/article/760  |y Kemija u industriji (Online) 
856 4 1 |y Digitalna.nsk.hr 
856 4 0 |u https://hrcak.srce.hr/243901  |y Hrčak